Thursday 23 May 2019

You have no chance. The xanthate decomposes when the pH is 4

One man asked: "Acid Flotation, anybody has experience in reverse flotation using acid flotation at pH 4.0 using sea water. Current standard use PAX, and glycol type frother.
The issue is an Iron Ore with sulphides as contaminants (Cu, Zn, Pb, S), Sulphur comes from Phyrrotite and Pyrite, so they want to reject all sulphides." More

I answered: "You have no chance. The xanthate decomposes when the pH is 4"